904L Stainless Steel Fittings & Flanges
904L (UNS N08904) is a high-alloy austenitic stainless steel with about 25% nickel, 4.5% molybdenum and 1.5% copper. It resists sulphuric acid, phosphoric acid and chloride pitting far better than 316L. Viraj Industrial Corporation manufactures and supplies 904L butt weld fittings to ASTM A403 WP904L and flanges and forged fittings to ASTM A182 F904L.
Specifications
Grades covered: UNS N08904.
| Product form or name | Specification and grade |
|---|---|
| Fittings | ASTM A403 WP904L |
| Flanges and forgings | ASTM A182 F904L |
| Pipe | ASTM A312 / B677 N08904 |
| Plate | ASTM A240 / B625 N08904 |
| Also known as | 1.4539, Alloy 904L |
Chemical composition
Composition limits in weight %, with related grades for comparison.
| Grade | UNS | C max % | Cr % | Ni % | Mo % | Other % |
|---|---|---|---|---|---|---|
| 904L | N08904 | 0.020 | 19.0–23.0 | 23.0–28.0 | 4.0–5.0 | Cu 1.0–2.0 |
| 304L | S30403 | 0.030 | 18.0–20.0 | 8.0–12.0 | — | — |
| 316L | S31603 | 0.030 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 | — |
| Duplex 2205 | S31803 | 0.030 | 21.0–23.0 | 4.5–6.5 | 2.5–3.5 | N 0.08–0.20 |
Typical minimum values from the ASTM product specifications. Limits differ slightly between plate, pipe, fittings and forgings, so confirm against the specification named on your order.
Mechanical properties
| Grade | Tensile strength min, MPa | Yield strength min, MPa | Elongation min, % |
|---|---|---|---|
| 904L | 490 | 220 | 35 |
Typical minimum values from the ASTM product specifications. Limits differ slightly between plate, pipe, fittings and forgings, so confirm against the specification named on your order.
Where it is used
Sulphuric and phosphoric acid plants, fertiliser production, flue gas scrubbers, seawater cooling, pulp and paper bleaching, and pharmaceutical process lines.
Questions and answers
What is 904L stainless steel?
904L is a low-carbon, high-alloy austenitic stainless steel, UNS N08904. It contains 19 to 23% chromium, 23 to 28% nickel, 4 to 5% molybdenum and 1 to 2% copper.
How is 904L different from 316L?
904L has roughly twice the nickel and molybdenum of 316L, and added copper. That gives much better resistance to sulphuric acid, chloride pitting and stress corrosion cracking. 316L has 10 to 14% nickel and 2 to 3% molybdenum.
Which ASTM specification covers 904L fittings and flanges?
Butt weld fittings are ordered to ASTM A403 grade WP904L, and flanges and forged fittings to ASTM A182 grade F904L.
Is 904L magnetic?
No. 904L is fully austenitic and stays non-magnetic, including after welding and forming.
Ask for a quotation
Send your size, grade and quantity. We reply with price, delivery time and test certificate details.